The following data have been obtained during a creep test of an asphalt paving mixture under a tensile stress of 700 Kpa and a temperature of 20 °C Times (s) 100 200 300 Creep (%) 0.6 0.8 1.0 The data refer to the period of secondary creep. What is the viscosity of the mixture?

Elements Of Electromagnetics
7th Edition
ISBN:9780190698614
Author:Sadiku, Matthew N. O.
Publisher:Sadiku, Matthew N. O.
ChapterMA: Math Assessment
Section: Chapter Questions
Problem 1.1MA
icon
Related questions
Question

Give me right solution.. please help me urgent

The following data have been obtained during a creep test of an asphalt paving
mixture under a tensile stress of 700 Kpa and a temperature of 20 °C
Times (s)
100
200
300
Creep (%)
0.6
0.8
1.0
The data refer to the period of secondary creep. What is the viscosity of the mixture?
Transcribed Image Text:The following data have been obtained during a creep test of an asphalt paving mixture under a tensile stress of 700 Kpa and a temperature of 20 °C Times (s) 100 200 300 Creep (%) 0.6 0.8 1.0 The data refer to the period of secondary creep. What is the viscosity of the mixture?
Expert Solution
steps

Step by step

Solved in 2 steps

Blurred answer
Knowledge Booster
Dimensional Analysis
Learn more about
Need a deep-dive on the concept behind this application? Look no further. Learn more about this topic, mechanical-engineering and related others by exploring similar questions and additional content below.
Similar questions
  • SEE MORE QUESTIONS
Recommended textbooks for you
Elements Of Electromagnetics
Elements Of Electromagnetics
Mechanical Engineering
ISBN:
9780190698614
Author:
Sadiku, Matthew N. O.
Publisher:
Oxford University Press
Mechanics of Materials (10th Edition)
Mechanics of Materials (10th Edition)
Mechanical Engineering
ISBN:
9780134319650
Author:
Russell C. Hibbeler
Publisher:
PEARSON
Thermodynamics: An Engineering Approach
Thermodynamics: An Engineering Approach
Mechanical Engineering
ISBN:
9781259822674
Author:
Yunus A. Cengel Dr., Michael A. Boles
Publisher:
McGraw-Hill Education
Control Systems Engineering
Control Systems Engineering
Mechanical Engineering
ISBN:
9781118170519
Author:
Norman S. Nise
Publisher:
WILEY
Mechanics of Materials (MindTap Course List)
Mechanics of Materials (MindTap Course List)
Mechanical Engineering
ISBN:
9781337093347
Author:
Barry J. Goodno, James M. Gere
Publisher:
Cengage Learning
Engineering Mechanics: Statics
Engineering Mechanics: Statics
Mechanical Engineering
ISBN:
9781118807330
Author:
James L. Meriam, L. G. Kraige, J. N. Bolton
Publisher:
WILEY